However, uranium leaching from ore on a large scale is widely practiced in the USA, South Africa, Canada and India. Insoluble tetravalent uranium is oxidized with a hot H 2 SO 4 /Fe 3+ solution to make soluble hexavalent uranium sulfate at pH and temperature 35°C (Crueger and Crueger, 1984). Contact Supplier